I am wondering if anybody has experience with using contact mask exposure for standard 1um 3612 resist coated on quartz substrates? The resist came out very clear on the quartz, so I am assuming the exposure time may be significantly different than the standard 1.2 s that I use with EVAligner. Any experience in this area would be appreciated.
Thank you,
Neil Dasgupta