- joey
On Mon, Mar 16, 2009 at 11:30 AM, Chris Kenney <kenney@slac.stanford.edu> wrote:
Hi Aaron,
Can you use the gaseous doping tubes: tylan5 and tylan6? Your
wafers must be CMOS-clean to use these tubes.
Chris
On Mon, 16 Mar 2009, Aaron Hryciw wrote:
Hello,would like to bring up my doping levels to >10?19 cm^-3 under my contacts.
Does anyone have experience with phosphorus-containing spin-on dopants? I
want to make an ohmic contact to n-type Si (P-doped, ~10^15 cm^-3), so I
I would greatly appreciate any advice you can give me regarding suppliers
and/or recipes that have produced good results at SNF.
Cheers!
? Aaron
--
Dr. Aaron Hryciw
Postdoctoral Scholar
Geballe Laboratory for Advanced Materials
Stanford University
476 Lomita Mall (04-490)
McCullough Building, Rm. 325
Stanford, CA 94305-4045
Tel.: (650) 723-5840
Fax.: (650) 736-1984